So, the latest test I did, using a more resin-friendly dye, making sure the containers, tools, my hands, everything were as surgically clean and dry as possible, cured beautifully with no bubbles or delamination.

Except. It made a big ol’ wrinkly fissure in the back which tells me that it was somehow too cold while curing in the oven for three hours. Really? Really?

IMG_2265[1]

Alumilite is supposed to be a pretty user-friendly resin. I don’t want to see one of the “difficult” ones!

This is the fifth or sixth time I’ve done this trial and I’m thoroughly sick of looking at these little pink squares. At least the silicone is working nicely so let’s do it. Let’s make mould for Clariel!

… right after I finish my coffee.

Happy Monday everybody!

Author: Ethan Kincaid

Ethan Kincaid was born in 1985 in Ontario, Canada. He graduated from Carleton University in Ottawa with a degree in Linguistics and a minor in Japanese Language. After finishing his education, he settled down there with his wife Kaitlyn and became a full-time writer. In 2011, he moved to Montreal and discovered its vibrant writing culture. In 2015, Ethan moved to Helsinki, Finland with his wife; he works as a creative craftsman and part time author. The greatest joy in his life lies in helping others find venues for their own personal expression.

Leave a Reply

Fill in your details below or click an icon to log in:

WordPress.com Logo

You are commenting using your WordPress.com account. Log Out /  Change )

Facebook photo

You are commenting using your Facebook account. Log Out /  Change )

Connecting to %s

%d bloggers like this: